| Element | Cu+Ag | Ag |
|---|---|---|
| Min (%) | 99.90 | 0.08 |
| Max (%) | Rem | 0.12 |
1. Silver elevates thermal softening to 350°C.
CuAg0.1% contains 0.1% silver which raises the softening point to 350°C without sacrificing 100% IACS electrical conductivity.
| Form | Range in mm | Tensile Strength in N/MM² | Elongation in % | Rockwell Hardness HRB | Conductivity% |
|---|---|---|---|---|---|
| Rotor Bar | Hard Drawn | 320-380 | 15 | 85-105 HB | 100 |
| Melting Point – Liquidus °C | 1083 |
| Electrical Conductivity% IACS at 20°C | 100 |
| Form | Size Dimensions |
|---|---|
| Rotor Bar | Tapered / Teardrop profiles up to 3500 mm length |